Stop in for a cup of coffee

Much bigger hole than I expected. (Go ahead Karl) Blow through from welding, not rust. Had to be there since installed. Not even sure why the were welding there since the flange appears to be factory welded. Not the way I like to do things, but certainly not a place I can weld. Hopefully it holds. Water based High heat metallic paste from JB Weld. Supposed to be good for manifold repairs. Needs to sit for a day before heated, so wifemobile goes to work today.