Header Paint

Reviving this old thread, used Rustolium Ultra Silver on a set of Dutra Slant Six Manifolds. The Dutra’s had been High Temp powder coated twice by Indy Powder Coat. The first trial did not last, neither did the second. Maybe it’s just me but I expected a premium high temp powder coat to look like new for more than one season. Especially since I paid for it twice.
So now I am trying the Rustolium Ultra.
Sprayed on easy enough. I let it set overnight then gave it the 450F oven today for a little over an hour. The coating sure looks nice. Will see what time and use does to it.