Speedmaster sale. It started

The flaw in the chamber is roughly 2mm deep. The walls in the hole in the chamber is pretty sealed off, so probably caused from an air bubble in the material when it was being cast.

They are much more shiny than my X-heads.... I'm like a woman with shiny jewelry lol.

View attachment 1715834332

View attachment 1715834334

View attachment 1715834335

View attachment 1715834336
I would have that hole welded closed..
Do like Pittsburgh said and JB some studs in the valve cover holes and run um like ya stole um.....