400 block number 1 cylinder thin area.

I think its cast issue. What i saw from plug holes and from waterpump holes water jacket looks very good for that old block, clean and not rusty. Wall thickness from opposite side of bore is nearly 0.300. And thats thickness about 40% of bore. Other bores are much more constant around.