I've heard people talk about "melonized" a fair amount recently, have never heard that until a few months ago, honestly. What exactly is that?
Salt bath nitriding. Results in a very hard, very slick, very thin "skin" on the part. You can get just about any alloy steel treated and on a per part basis it isn't very expensive but doing one offs there is usually a setup fee and it's not so economical. They've been doing custom rifle barrels and it is $100-$150 per. Barrels last MUCH longer.