Some paint questions for the guys who know paint

2 sessions of polyester primer, 2 sessions of dry sanding
2 more rounds of K38 high build and 2 more times dry sand
1 last round of K36, and then 2 more sessions of wet sanding

It's a lot of work, but it's straighter than an arrow. All this is based on your metal, and that your mud work is straight.


It isn't the body, I work it until it's straight as a die, it's the clear, most people I've talked to get the dreaded Urethane Wave, even when you flow coat. Not really on hoods and other flat areas where I guess it can flow out better. What type of clear do you use? I use Dupont Chroma Premier, very high solids I guess, probably a contributing factor